一、模具專業英語
出(chū)模: mould unloading, mold stripping
出模角 : Draft Angle
出模方向: The direction of the mold Mold Parting Direction
入水:gate
進入位:gate locations
水口形式(shì):gate type
大水口(kǒu):edge gate
細水口:pin-point gate
水口大小:gate size
轉水口:switching runner/gate
唧嘴口徑:sprue diameter
二、流道: runner
熱流道:hot runner,hot manifold
熱嘴冷流道: hot sprue/cold runner
唧嘴直流: direct sprue gate
圓形流道:round(full/half runner
流道電腦分析:mold flow analysis
流道平(píng)衡: runner balance
熱嘴:hot sprue
熱流道板:hot manifold
發熱管:cartridge heater
探針: thermocouples
插頭:connector plug
插座:connector socket
密封/封料:seal
三、運水:water line
喉塞:line lpug
喉管:tube
塑膠管:plastic tube
快速接頭:jiffy quick connector plug/socker
四、模具零件:mold components
三板模:3-plate mold
二板模:2-plate mold
邊釘(dìng)/導邊:l eader pin/guide pin
邊司/導套:bushing/guide bushing
中托司:shoulder guide bushing
中托邊L:guide pin
頂針板:ejector retainner plate
托板(bǎn):support plate
螺絲:screw
管釘:dowel pin
開模槽(cáo):ply bar scot
內模管位:core/cavity inter-lock
頂針:ejector pin
司筒:ejector sleeve
司(sī)筒針(zhēn):ejector pin
推板:stripper plate
縮嗬:movable core,return core core puller
扣機(尼龍拉勾):nylon latch lock
斜頂:lifter
模胚(架):mold base
上內模:cavity insert
下內(nèi)模:core insert
行位(滑塊):slide
鑲(xiāng)件:insert
壓座/斜雞:wedge
耐磨板/油板:wedge wear plate
壓條:plate
撐頭: support pillar
唧嘴:sprue bushing
擋板:stop plate
定位圈:locating ring
鎖扣:latch
扣雞:parting lock set
推(tuī)杆:push bar
栓打螺絲:S.H.S.B
頂板:eracuretun
活(huó)動臂:lever arm
分流錐:spure sperader
水(shuǐ)口司: bush
垃圾釘:stop pin
隔片:buffle
彈弓柱:spring rod
彈弓: die spring
中托司:ejector guide bush
中托(tuō)邊:ejector guide pin
鑲針:pin
銷子:dowel pin
波子彈弓:ball catch
模具成形不良用語英漢對照
aberration 色差
atomization 料紋
bite 咬入(rù)
blacking hole 塗料孔(鑄疵)
blacking scab 塗料疤
blister 起泡
blooming 起霜
low hole 破孔
blushing 泛白
body wrinkle 側壁皺紋
breaking-in 冒口帶肉
bubble 膜泡
burn mark 糊斑
burr 毛邊
camber 翹曲
cell 氣泡
center buckle 表麵中部波皺
check 細裂(liè)痕
checking 龜裂
chipping 修整表麵缺陷
clamp-off 鑄件凹痕
collapse 塌陷
color mottle 色斑
corrosion 腐蝕
crack 裂痕
crazing 碎裂
crazing 龜(guī)裂
deformation 變形
edge 切邊碎片
edge crack 裂邊
fading 退色
filler speak 填充料斑
fissure 裂紋
flange wrinkle 凸緣起皺
flaw 刮傷
flow mark 流痕
galling 毛邊(biān)
glazing 光滑
gloss 光澤
grease pits 汙斑
grinding defect 磨痕
haircrack 發(fā)裂
haze 霧度
incrustation 水鏽
indentation 壓痕
internal porosity 內部氣孔
mismatch 偏模(mó)
mottle 斑點(diǎn)
necking 縮頸
nick 割痕
orange peel 橘皮狀表(biǎo)麵缺陷
overflow 溢流
peeling 剝(bāo)離
pit 坑
pitting corrosion 點狀腐蝕
plate mark 模板印痕(hén)
pock 麻點
pock mark 痘斑
resin streak 樹脂流紋
resin wear 樹脂脫落
riding 凹陷
sagging 鬆垂
saponification 皂化
scar 疤痕
scrap 廢料
scrap jam 廢料阻塞
scratch 刮傷(shāng)/劃痕
scuffing 深衝表麵劃傷
seam 裂痕
shock line 模口擠痕
short shot 充填不足
shrinkage pool 凹孔(kǒng)
sink mark 凹痕
skin inclusion 表皮折疊
straightening 矯直
streak 條狀痕
surface check 表麵裂痕
surface roughening 橘(jú)皮狀表皮皺折
surging 波動
sweat out 冒汗
torsion 扭曲(qǔ)
warpage 翹曲
waviness 波(bō)痕
webbing 熔塌
weld mark 焊痕
whitening 白化
wrinkle 皺(zhòu)紋